Abstract

For improving the wear resistance, thick silicon doped hydrogenated amorphous carbon (a-SiC:H) coatings were deposited on cold working tool steels by plasma-enhanced chemical vapor deposition (PECVD) technology. The increase of the acetylene (C2H2) flow rate distinctly tuned the microstructure of a-SiC:H coatings, including an increase in the coating thickness (>15 µm), a decrease in the silicon content, a greater sp2/sp3 ratio, and higher degree of graphitization. The highest hardness of 19.61 GPa and the greatest critical load of 50.7 N were obtained. The coating showed low wear rate against different friction pairs and presented excellent abrasive wear resistance at high applied load and the wear rate decreased with increasing loads, which exhibited an outstanding application prospect in cold working tool steels.

References

1.
Toboła
,
D.
,
Brostow
,
W.
,
Czechowski
,
K.
, and
Rusek
,
P.
,
2017
, “
Improvement of Wear Resistance of Some Cold Working Tool Steels
,”
Wear
,
382–383
, pp.
29
39
.
2.
Rottger
,
A.
,
Weber
,
S. L.
,
Theisen
,
W.
,
Rajasekaran
,
B.
, and
Vaβen
,
R.
,
2009
, “
High Velocity Oxy Fuel Spraying of Cold Work Tool Steels—A Novel Approach to Thick Coatings for Wear Protection Applications
,”
Adv. Eng. Mater.
,
11
(
12
), pp.
1015
1022
.
3.
Zappelino
,
B. F.
,
de Almeida
,
E. A. D.
,
Krelling
,
A. P.
,
da Costa
,
C. E.
,
Fontana
,
L. C.
, and
Milan
,
J. C. G.
,
2020
, “
Tribological Behavior of Duplex-Coating on Vanadis 10 Cold Work Tool Steel
,”
Wear
,
442–443
, p.
203133
.
4.
Ramiez
,
G.
,
Jimenez-Pique
,
E.
,
Mestra
,
A.
,
Vilaseca
,
M.
,
Casellas
,
D.
, and
Llanes
,
L.
,
2015
, “
A Comparative Study of the Contact Fatigue Behavior and Associated Damage Micromechanisms of TiN- and WC:H-Coated Cold-Work Tool Steel
,”
Tribol. Int.
,
88
, pp.
263
270
.
5.
Kumar
,
S.
,
Maity
,
S. R.
, and
Patnaik
,
L.
,
2020
, “
Effect of Heat Treatment and TiN Coating on AISI O1 Cold Work Tool Steel
,”
Mater. Today: Proc.
,
26
(
2
), pp.
685
688
.
6.
Farayibi
,
P. K.
,
Blüm
,
M.
, and
Weber
,
S.
,
2020
, “
Densification of a High Chromium Cold Work Tool Steel Powder in Different Atmospheres by SLPS: Microstructure, Heat Treatment and Micromechanical Properties
,”
Mater. Sci. Eng. A
,
777
, p.
139053
.
7.
Maatta
,
A.
,
Vuoristo
,
P.
, and
Mantyla
,
T.
,
2001
, “
Friction and Adhesion of Stainless Steel Strip Against Tool Steels in Unlubricated Sliding With High Contact Load
,”
Tribol. Int.
,
34
(
11
), pp.
779
786
.
8.
de Melo Silva
,
W.
,
Martins
,
P. S.
,
de Carvalho
,
V. E.
,
da Cruz
,
N. C.
,
Claudino
,
E.
, and
Carneiro
,
J. R. G.
,
2020
, “
Improving Precision in Aluminum Alloy Machining Due to the Application of Diamond-Like Carbon Thin Film
,”
ASME J. Tribol.
,
143
(
7
), p.
071403
.
9.
Wang
,
Y.
,
Xu
,
J.
,
Zhang
,
J.
,
Chen
,
Q.
,
Ootani
,
Y.
,
Higuchi
,
Y.
,
Ozawa
,
N.
,
Martin
,
J. M.
,
Adachi
,
K.
, and
Kubo
,
M.
,
2018
, “
Tribochemical Reactions and Graphitization of Diamond-Like Carbon Against Alumina Give Volcano-Type Temperature Dependence of Friction Coefficients: A Tight-Binding Quantum Chemical Molecular Dynamics Simulation
,”
Carbon
,
133
, pp.
350
357
.
10.
Xu
,
J.
,
Duan
,
Z.
,
Qiao
,
L.
,
Chai
,
L.
,
Chen
,
Z.
,
Guo
,
D.
,
Wang
,
P.
, and
Liu
,
W.
,
2019
, “
Nonuniform Transitions of Heavy-Ion Irradiated a-C:H Films: Structure and Antiwear Property Degradation Analysis
,”
Carbon
,
146
, pp.
200
209
.
11.
Wang
,
Y.
,
Xu
,
J.
,
Ootani
,
Y.
,
Ozawa
,
N.
,
Adachi
,
K.
, and
Kubo
,
M.
,
2019
, “
Proposal of a New Formation Mechanism for Hydrogenated Diamond-Like Carbon Transfer Films: Hydrocarbon-Emission-Induced Transfer
,”
Carbon
,
154
, pp.
7
12
.
12.
Dearnley
,
P. A.
,
Elwafi
,
A. M.
,
Chittenden
,
R. J.
, and
Barton
,
D. C.
,
2014
, “
Wear and Friction of Diamondlike-Carbon Coated and Uncoated Steel Roller Bearings Under High Contact Pressure Oil Lubricated Rolling/Sliding Conditions
,”
ASME J. Tribol.
,
136
(
2
), p.
021101
.
13.
Bootkul
,
D.
,
Supsermpol
,
B.
,
Saenphinit
,
N.
,
Aramwit
,
C.
, and
Intarasiri
,
S.
,
2014
, “
Nitrogen Doping for Adhesion Improvement of DLC Film Deposited on Si Substrate by Filtered Cathodic Vacuum Arc (FCVA) Technique
,”
Appl. Surf. Sci.
,
310
(
SI
), pp.
284
292
.
14.
Hilbert
,
J.
,
Mangolini
,
F.
,
McClimon
,
J. B.
,
Lukes
,
J. R.
, and
Carpick
,
R. W.
,
2018
, “
Si Doping Enhances the Thermal Stability of Diamond-Like Carbon Through Reductions in Carbon-Carbon Bond Length Disorder
,”
Carbon
,
131
, pp.
72
78
.
15.
Lee
,
C. S.
,
Lee
,
K. R.
,
Eun
,
K. Y.
,
Yoon
,
K. H.
, and
Han
,
J. H.
,
2002
, “
Structure and Properties of Si Incorporated Tetrahedral Amorphous Carbon Films Prepared by Hybrid Filtered Vacuum Arc Process
,”
Diamond Relat. Mater.
,
11
(
2
), pp.
198
203
.
16.
Li
,
X. W.
,
Joe
,
M. W.
,
Wang
,
A. Y.
, and
Lee
,
K. R.
,
2013
, “
Stress Reduction of Diamond-Like Carbon by Si Incorporation: A Molecular Dynamics Study
,”
Surf. Coat. Technol.
,
228
(
1
), pp.
S190
S193
.
17.
Crespi
,
A. E.
,
Leidens
,
L. M.
,
Antunes
,
V.
,
Perotti
,
B. L.
,
Michels
,
A. F.
,
Alvarez
,
F.
, and
Figueroa
,
C. A.
,
2019
, “
Substrate Bias Voltage Tailoring the Interfacial Chemistry of a-SiCx:H: A Surprising Improvement in Adhesion of a-C:H Thin Films Deposited on Ferrous Alloys Controlled by Oxygen
,”
ACS Appl. Mater. Interfaces
,
11
(
19
), pp.
18024
18033
.
18.
Wang
,
J. J.
,
Pu
,
J. B.
,
Zhang
,
G. G.
, and
Wang
,
L. P.
,
2013
, “
Tailoring the Structure and Property of Silicon-Doped Diamond-Like Carbon Films by Controlling the Silicon Content
,”
Surf. Coat. Technol.
,
235
, pp.
326
332
.
19.
Lee
,
K. R.
,
Kim
,
M. G.
,
Cho
,
S. J.
,
Yong Eun
,
K.
, and
Seong
,
T. Y.
,
1997
, “
Structural Dependence of Mechanical Properties of Si Incorporated Diamond-Like Carbon Films Deposited by RF Plasma-Assisted Chemical Vapour Deposition
,”
Thin Solid Films
,
308–309
, pp.
263
267
.
20.
Wang
,
J.
,
Pu
,
J.
,
Zhang
,
G.
, and
Wang
,
L.
,
2013
, “
Interface Architecture for Superthick Carbon-Based Films Toward Low Internal Stress and Ultrahigh Load-Bearing Capacity
,”
ACS Appl. Mater. Interfaces
,
5
(
11
), pp.
5015
5024
.
21.
Podgornik
,
B.
, and
Leskovšek
,
V.
,
2015
, “
Wear Mechanisms and Surface Engineering of Forming Tools
,”
Mater. Tehnol.
,
49
(
3
), pp.
313
324
.
22.
Barber
,
J. R.
, and
Ciavarella
,
M.
,
2000
, “
Contact Mechanics
,”
Int. J. Solids Struct.
,
37
(
1–2
), pp.
29
43
.
23.
Shiri
,
S.
,
Ashtijoo
,
P.
,
Odeshi
,
A.
, and
Yang
,
Q.
,
2016
, “
Evaluation of Stoney Equation for Determining the Internal Stress of DLC Thin Films Using an Optical Profiler
,”
Surf. Coat. Technol.
,
308
, pp.
98
100
.
24.
Jiang
,
L. H.
,
Tan
,
X. Y.
,
Xiao
,
T.
, and
Xiang
,
P.
,
2017
, “
The Influence of Methane Flow Rate on Microstructure and Surface Morphology of a-SiC:H Thin Films Prepared by Plasma Enhanced Chemical Vapor Deposition Technique
,”
Thin Solid Films
,
622
, pp.
71
77
.
25.
Jiang
,
J.
,
Wang
,
Y.
,
Du
,
J.
,
Yang
,
H.
, and
Hao
,
J.
,
2016
, “
Properties of a-C:H:Si Thin Films Deposited by Middle-Frequency Magnetron Sputtering
,”
Appl. Surf. Sci.
,
379
, pp.
516
522
.
26.
Zhang
,
H. Y.
,
Liu
,
L. X.
,
Wang
,
Y. L.
,
Ma
,
H. T.
, and
Liu
,
F. X.
,
2007
, “
Structure and Mechanical Performance of Nitrogen Doped Diamond-Like Carbon Films
,”
J. Mater. Sci. Technol.
,
23
(
4
), pp.
491
494
.
27.
Bendavid
,
A.
,
Martin
,
P. J.
,
Comte
,
C.
,
Preston
,
E. W.
,
Haq
,
A. J.
,
Magdon Ismail
,
F. S.
, and
Singh
,
R. K.
,
2007
, “
The Mechanical and Biocompatibility Properties of DLC-Si Films Prepared by Pulsed DC Plasma Activated Chemical Vapor Deposition
,”
Diamond Relat. Mater.
,
16
(
8
), pp.
1616
1622
.
28.
Yan
,
X.
,
Xu
,
T.
,
Chen
,
G.
,
Yang
,
S.
, and
Liu
,
H.
,
2004
, “
Study of Structure, Tribological Properties and Growth Mechanism of DLC and Nitrogen-Doped DLC Films Deposited by Electrochemical Technique
,”
Appl. Surf. Sci.
,
236
(
1–4
), pp.
328
335
.
29.
Qiang
,
L.
,
Zhang
,
B.
,
Zhou
,
Y.
, and
Zhang
,
J.
,
2013
, “
Improving the Internal Stress and Wear Resistance of DLC Film by Low Content Ti Doping
,”
Solid State Sci.
,
20
, pp.
17
22
.
30.
Zhang
,
T. F.
,
Wan
,
Z. X.
,
Ding
,
J. C.
,
Zhang
,
S.
,
Wang
,
Q. M.
, and
Kim
,
K. H.
,
2018
, “
Microstructure and High-Temperature Tribological Properties of Si-Doped Hydrogenated Diamond-Like Carbon Films
,”
Appl. Surf. Sci.
,
435
, pp.
963
973
.
31.
Ferrari
,
A. C.
, and
Robertson
,
J.
,
2000
, “
Interpretation of Raman Spectra of Disordered and Amorphous Carbon
,”
Phys. Rev. B
,
61
(
20
), pp.
14095
14107
.
32.
Gago
,
R.
,
Vinnichenko
,
M.
,
Jäger
,
H. U.
,
Belov
,
A. Y.
,
Jiménez
,
I.
,
Huang
,
N.
,
Sun
,
H.
, and
Maitz
,
M. F.
,
2005
, “
Evolution of sp2 Networks With Substrate Temperature in Amorphous Carbon Films: Experiment and Theory
,”
Phys. Rev. B
,
72
(
1
).
33.
Shi
,
X.
,
Liskiewicz
,
T. W.
,
Beake
,
B. D.
,
Chen
,
J.
, and
Wang
,
C.
,
2020
, “
Tribological Performance of Graphite-Like Carbon Films With Varied Thickness
,”
Tribol. Int.
,
149
(
105586
).
34.
Huang
,
L.
,
Yuan
,
J.
,
Li
,
C.
, and
Hong
,
D.
,
2018
, “
Microstructure, Tribological and Cutting Performance of Ti-DLC/α-C:H Multilayer Film on Cemented Carbide
,”
Surf. Coat. Technol.
,
353
, pp.
163
170
.
35.
Guo
,
C. Q.
,
Lin
,
S. S.
,
Gao
,
D.
,
Shi
,
Q.
,
Wei
,
C. B.
,
Dai
,
M. J.
,
Su
,
Y. F.
, et al
,
2020
, “
Modulation of Si on Microstructure and Tribo-Mechanical Properties of Hydrogen-Free DLC Films Prepared by Magnetron Sputtering
,”
Appl. Surf. Sci.
,
509
.
36.
Wu
,
M.
,
Tian
,
X.
,
Li
,
M.
,
Gong
,
C.
, and
Wei
,
R.
,
2016
, “
Effect of Additional Sample Bias in Meshed Plasma Immersion Ion Deposition (MPIID) on Microstructural, Surface and Mechanical Properties of Si-DLC Films
,”
Appl. Surf. Sci.
,
376
, pp.
26
33
.
37.
Liu
,
C.
,
Lin
,
Y.
,
Zhou
,
Z.
, and
Li
,
K.-Y.
,
2017
, “
Dual Phase Amorphous Carbon Ceramic Achieves Theoretical Strength Limit and Large Plasticity
,”
Carbon
,
122
, pp.
276
280
.
38.
Li
,
X. D.
, and
Bhushan
,
B.
,
1999
, “
Micro/Nanomechanical and Tribological Characterization of Ultrathin Amorphous Carbon Coatings
,”
J. Mater. Res.
,
14
(
6
), pp.
2328
2337
.
39.
Scharf
,
T. W.
, and
Singer
,
I. L.
,
2009
, “
Role of the Transfer Film on the Friction and Wear of Metal Carbide Reinforced Amorphous Carbon Coatings During Run-in
,”
Tribology Letter
,
36
(
1
), pp.
43
53
.
40.
Zhou
,
S.
,
Wang
,
L.
,
Lu
,
Z.
,
Ding
,
Q.
,
Wang
,
S. C.
,
Wood
,
R. J. K.
, and
Xue
,
Q.
,
2012
, “
Tailoring Microstructure and Phase Segregation for Low Friction Carbon-Based Nanocomposite Coatings
,”
J. Mater. Chem.
,
22
(
31
), p.
15782
.
41.
Sui
,
X.
,
Wang
,
X.
,
Zhang
,
S.
,
Yan
,
M.
,
Li
,
W.
,
Hao
,
J.
, and
Liu
,
W.
,
2020
, “
Nano-Twisted Double Helix Carbon Debris Improves the Wear Resistance of Ultra-Thick Diamond-Like Carbon Coatings
,”
Adv. Mater. Interfaces
,
7
(
20
), p.
200857
.
42.
Chouquet
,
C.
,
Gerbaud
,
G.
,
Bardet
,
M.
,
Barrat
,
S.
,
Billard
,
A.
,
Sanchette
,
F.
, and
Ducros
,
C.
,
2010
, “
Structural and Mechanical Properties of a-C:H and Si Doped a-C:H Thin Films Grown by LF-PECVD
,”
Surf. Coat. Technol.
,
204
(
9–10
), pp.
1339
1346
.
43.
Cui
,
L.
,
Lu
,
Z.
, and
Wang
,
L.
,
2013
, “
Toward Low Friction in High Vacuum for Hydrogenated Diamondlike Carbon by Tailoring Sliding Interface
,”
ACS Appl. Mater. Interfaces
,
5
(
13
), pp.
5889
5893
.
44.
Aghababaei
,
R.
, and
Zhao
,
K.
,
2021
, “
Micromechanics of Material Detachment During Adhesive Wear: A Numerical Assessment of Archard's Wear Model
,”
Wear
,
476
.
45.
Wang
,
L.
,
Bai
,
L.
,
Lu
,
Z.
,
Zhang
,
G.
, and
Wu
,
Z.
,
2013
, “
Influence of Load on the Tribological Behavior of a-C Films: Experiment and Calculation Coupling
,”
Tribology Letter
,
52
(
3
), pp.
469
475
.
46.
Hasselbruch
,
H.
,
Herrmann
,
M.
,
Mehner
,
A.
,
Kuhfuss
,
B.
, and
Zoch
,
H. W.
,
2017
, “
Incremental Dry Forging—Interaction of W-DLC Coatings and Surface Structures for Rotary Swaging Tools
,”
Procedia Manuf.
,
8
, pp.
541
548
.
47.
Czyzniewski
,
A.
,
2012
, “
Optimising Deposition Parameters of W-DLC Coatings for Tool Materials of High Speed Steel and Cemented Carbide
,”
Vacuum
,
86
(
12
), pp.
2140
2147
.
48.
Çalışkan
,
H.
,
2014
, “
Effect of Test Parameters on the Micro-Abrasion Behavior of PVD CrN Coatings
,”
Measurement
,
55
, pp.
444
451
.
49.
Makowski
,
S.
,
Schaller
,
F.
,
Weihnacht
,
V.
,
Englberger
,
G.
, and
Becker
,
M.
,
2017
, “
Tribochemical Induced Wear and Ultra-Low Friction of Superhard ta-C Coatings
,”
Wear
,
392–393
, pp.
139
151
.
You do not currently have access to this content.